Architectural Ceramics
Revision as of 15:43, 15 May 2011 by Ricon (talk | contribs) (Created page with "<bibimport/> <br> Author: Hans-Jürgen Schwarz <br> Back to Decay pattern <br> == Abstract == Für Baukeramik typische Schadensbilder werden vorgestellt...")
<bibimport/>
Author: Hans-Jürgen Schwarz
Back to Decay pattern
Abstract
Für Baukeramik typische Schadensbilder werden vorgestellt und anhand von Abbildungen erläutert.
Decay Pattren on Architectural Ceramics
Ziegelschäden
Salt-induced damage to bricks are common.
Damage to bricks can look like this:
Scaling(?)
Figure 3: Photomicrograph as Fig 2 but with crossed polarisers. It is clearly seen that the plaster is both responsible for the damage and on the other hand, he acts in this case as a kind of glue that holds together the broken brick pieces. With the removal of the original plaster the brick material would be lost.